Patent References 3180854 3384623 3393243 3427256 3427334 3427335 3483167 3829505 Polyethers and method for making the same Process for preparing polyols InventorsAssigneeApplicationNo. 10158988 filed on 05/30/2002US Classes:528/55, Material contains at least one metal atom528/56, Material contains a transition metal atom528/57, Material contains at least one group IA or group IIA metal atom528/58, Material contains at least one atom of tin528/61, With organic nitrogen reactant which contains two NH, =NH, or HNH groups528/64, Organic NH, =NH or HNH nitrogen reactant contains a carbocyclic or aromatic ring528/906, FIBER OR ELASTOMER PREPARED FROM AN ISOCYANATE REACTANT568/618, Preparing from organic hydroxy containing compound (H of -OH may be replaced by a Group IA or IIA light metal)544/398, Chalcogen attached indirectly to the piperazine ring by nonionic bonding521/159, N=C=X reactant having at least two C-NH-C(=X)- groups, e.g., prepolymers, etc.536/120, Ethers252/182.27, Reactant contains ether linkage524/591Water DNRMExaminersPrimary: Gorr, RachelAttorney, Agent or FirmForeign Patent References
International ClassC08G018/16AbstractSegmented polyurethane/ureas useful for the production of spandex, particularly spandex fibers, are made from isocyanate-terminated prepolymers formed by reacting excess isocyanate with an isocyanate-reactive component satisfying specified compositional requirements in the presence of a catalyst which promotes linear polymerization but does not cause degradation of the polymer. Suitable catalysts include metal salts of organic fatty acids and/or of naphthenic acid. The isocyanate-reactive component includes at least 10 equivalent percent of a polyoxypropylene diol having a number average molecular weight of at least about 1500 Da and an average unsaturation level less than or equal to 0.03 meq/g and up to 90 equivalent percent of a polytetramethylene glycol having a number average molecular weight of at least 200 Da.Other References
|
| ||||||||||||||