Abrasive grain containing alumina and zirconia

Patent 5551963 Issued on September 3, 1996. Estimated Expiration Date: Icon_subject November 6, 2015. Estimated Expiration Date is calculated based on simple USPTO term provisions. It does not account for terminal disclaimers, term adjustments, failure to pay maintenance fees, or other factors which might affect the term of a patent.

Patent References

3454385

3891408

Co-fused alumina-zirconia alloy abrasive containing magnesium oxide
Patent #: 4126429
Issued on: 11/21/1978
Inventor: Watson

Non-fused aluminum oxide-based abrasive mineral
Patent #: 4314827
Issued on: 02/09/1982
Inventor: Leitheiser ,   et al.

Alumina sintered products and process for their production
Patent #: 4331627
Issued on: 05/25/1982
Inventor: Yamamoto ,   et al.

High silica faujasite polymorph - CSZ-3 and method of synthesizing
Patent #: 4333859
Issued on: 06/08/1982
Inventor: Vaughan ,   et al.

Alumina-zirconia abrasive
Patent #: 4457767
Issued on: 07/03/1984
Inventor: Poon ,   et al.

Articles containing non-fused aluminum oxide-based abrasive mineral
Patent #: 4518397
Issued on: 05/21/1985
Inventor: Leitheiser ,   et al.

Process for durable sol-gel produced alumina-based ceramics, abrasive grain and abrasive products
Patent #: 4744802
Issued on: 05/17/1988
Inventor: Schwabel

Abrasive grits formed of ceramic containing oxides of aluminum and yttrium, method of making and using the same and products made therewith
Patent #: 4770671
Issued on: 09/13/1988
Inventor: Monroe ,   et al.

More ...

Inventor

Assignee

Application

No. 554033 filed on 11/06/1995

US Classes:

51/307, WITH INORGANIC MATERIAL51/309Metal or metal oxide

Examiners

Primary: Jones, Deborah

Foreign Patent References

  • 394850 AT 12/23/1991
  • 0236507A1 EP 09/23/1987
  • 256182A1 EP 02/23/1988
  • 0293164 EP 11/23/1988
  • 0293163 EP 11/23/1988
  • 0368837 EP 05/23/1990
  • 408771A1 EP 01/23/1991
  • 0435677A2 EP 07/23/1991
  • 0441640A2 EP 08/23/1991
  • 4097942 JP 03/23/1992
  • WO92/01646 WO 02/23/1992

International Class

B24D 003/34

Abstract

A method of preparing preferred abrasive grain includes: preparing a dispersion including alpha alumina oxide monohydrate and zirconia sol therein; converting the dispersion to base grit material; and sintering the base grit to form abrasive grains. The presence of the zirconia sol within the dispersion from which the base grits are formed provides an improved abrasive grain. The improved abrasive grain are useful in abrasive products.

Other References

  • "High Toughness Ce-TZP/Al2 O3 Cermaics with Improved Hardness and Strength," R. A. Cutler et al., J. Am. Ceram. Soc., 74, No. 1. (1991), pp. 179-186
  • "The Hardness, Stiffness and Toughness of Diphasic Abrasive Materials Prepared by Sol-Gel Techniques," E. Breval et al., Mat. Res. Bull., 20, No. 4 (1985), pp. 413-429
  • "Use of Sintered Ceramic Aluminum Oxides in Vitrified Bonded Wheels," S. C. Yoon et al., SME Technical Paper EM90-360, (1990)
  • "Chemical Processing of Ceramics," D. R. Ulrich, C&EN Special Report, Jan. 1, 1990, pp. 28-40
  • "Influence of Small ZrO2 Additions on the Microstructure and Mechanical Properties of Al2 O3," Hori et al., Advances in Ceramics, Science and Technology of Zirconia III, 24A, The American Ceramic Society, (1988), pp. 423-42
PatentsPlus Images
Enhanced PDF formats
loading...
PatentsPlus: add to cart
PatentsPlus: add to cartSearch-enhanced full patent PDF image
$9.95more info
PatentsPlus: add to cart
PatentsPlus: add to cartIntelligent turbocharged patent PDFs with marked up images
$16.95more info
 
Sign InRegister
Username  
Password   
forgot password?