Patent 5420186 Issued on May 30, 1995. Estimated Expiration Date: January 26, 2013. Estimated Expiration Date is calculated based on simple USPTO term provisions. It does not account for terminal disclaimers, term adjustments, failure to pay maintenance fees, or other factors which might affect the term of a patent.
524/236, Trivalent or tetravalent nitrogen atom other than unsubstituted ammonium524/394, Oxygen atom or metal atom DNRM, e.g., metal stearate, etc.524/398, Transition metal atom (atomic no. 21-29, 39-47, 57-79)524/399, Heavy metal or aluminum (atomic no. 13, 30-33, 48-51, 80-83)524/400, Group IIA metal (Be, Mg, Ca, Sr, Ba)524/714, N-containing organic compound excluding unsubstituted ammonium as sole nitrogen in DNRM524/779, Elemental metal or metal compound not containing silicon DNRM524/780, Heavy metal524/786Al
In an active hydrogen-containing B-side composition for reaction with a polyisocyanate-containing A-side composition to make a polyurethane or polyurethaneurea elastomer by reaction injection molding, the improvement which comprises a mold release composition consisting essentially of (1) a liquid quaternary ammonium salt and (2) a metal salt of a fatty acid.