U.S. patents available from 1976 to present.
U.S. patent applications available from 2005 to present.

Icon_funbox Bizarre Patents

Patent No. 5443036

Method of exercising a cat

A method for inducing cats to exercise consists of directing a beam of invisible light produced by a hand-held laser apparatus onto the floor or wall.

Newsletter  PatentStorm News

Make the Most of Our Site

See this month's Top Inventors and Most Cited Patents.

Stay on top of the latest innovations by subscribing to an RSS feed.

Registered users: Manage your profile.

 

Class 420/584.1 - Nickel containing


Subclass of Class 420 - Alloys or metallic compositions
Definition: Alloy, or metallic composition which additionally contains nickel.
No. of applications: 21
Last issue date: 03/01/2012


Application No.Application TitleIssue Date
20120051963NICKEL-IRON-BASE ALLOY AND PROCESS OF FORMING A NICKEL-IRON-BASE ALLOY
A nickel-iron-base alloy has by weight about 0.06% to about 0.09% C, about 35% to about 37% Fe, about 12.0% to about 16.5% Cr, about 1.0% to about 2.0% Al, about 1.0% to about 3.0% Ti, about 1.5% to about 3.0% W, up to about 5.0% Mo, up to about 0.75% Nb, up to about 0....
03/01/2012
20110311390STEEL MATERIAL COMPOSITION FOR PRODUCING PISTON RINGS AND CYLINDER SLEEVES
The invention relates to a steel material composition, in particular for producing piston rings and cylinder sleeves, containing the following elements in the given fractions in relation to 100% by weight of the steel material: 0.5-1.2% by weight C, 6.0-20.0% by weight ...
12/22/2011
20110248071AUSTENITIC WELDING MATERIAL, AND PREVENTIVE MAINTENANCE METHOD FOR STRESS CORROSION CRACKING AND PREVENTIVE MAINTENANCE METHOD FOR INTERGRANULAR CORROSION, USING SAME
Disclosed is an austenitic welding material which contains C: 0.01 wt % or less, Si: 0.5 wt % or less, Mn: 0.5 wt % or less, P: 0.005 wt % or less, S: 0.005 wt % or less, Ni: 15 to 40 wt %, Cr: 20 to 30 wt %, N: 0.01 wt % or less, 0: 0.01 wt % or less, and the balance o...
10/13/2011
20110226459MATERIAL FOR JOINING AND PRODUCT PRODUCED THEREWITH
The invention relates to an iron-based brazing material comprising a brazing alloy, which alloy comprises: from about 9 wt % to about 30 wt % Cr, from about 5 wt % to about 25 wt % Ni, from about 0 wt % to about 9 wt % Mo, from about 0 wt % to about 5 wt % Mn, from abou...
09/22/2011
20110192127STAINLESS STEEL FOR FILTER APPLICATIONS
A filter comprising a porous sintered stainless steel is provided. The filter includes 10-30% chromium, 5-25% nickel, 0.5-3% manganese; 1-4% silicon, and 0-3% molybdenum with the remainder being iron and inevitable impurities. The sintered steel has a density less than ...
08/11/2011
20110088819AUSTENITIC HEAT RESISTANT ALLOY, HEAT RESISTANT PRESSURE MEMBER COMPRISING THE ALLOY, AND METHOD FOR MANUFACTURING THE SAME MEMBER
An austenitic heat resistant alloy, which comprises by mass percent, C: over 0.02 to 0.15%, Si≦2%, Mn≦3%, P≦0.03%, S≦0.01%, Cr: 28 to 38%, Ni: over 40 to 60%, Co≦20% (including 0%), W over 3 to 15%, Ti: 0.05 to 1.0%, Zr: 0.005 to 0.2%, Al: 0.01 to 0.3%, N≦0....
04/21/2011
20110041967Eutectic Alloys of the Type FE 25-35 NI 15-25 MN 30-40 AL 10-20 M 0-5 and Methods for Production Thereof
Alloys, formed by a eutectic transformation of the type Fe25-35 Ni15-25 Mn30-40 Al10-20 MO-5, are disclosed. M is selected from chromium, molybdenum, carbon and combinations thereof. The alloys have high strength and ductility. The alloys are prepared from readily avail...
02/24/2011
20110008714LOW-COST MANGANESE-STABILIZED AUSTENITIC STAINLESS STEEL ALLOYS, BIPOLAR PLATES COMPRISING THE ALLOYS, AND FUEL CELL SYSTEMS COMPRISING THE BIPOLAR PLATES
Corrosion resistant, manganese-stabilized austenitic stainless steels with a low nickel content are used in bipolar plates, methods for fabricating the bipolar plates, and polymer electrolyte membrane (PEM) fuel cells comprising the bipolar plates. The bipolar plates ar...
01/13/2011
20100303669Cast Heat-Resistant Austenitic Steel with Improved Temperature Creep Properties and Balanced Alloying Element Additions and Methodology for Development of the Same
The present invention addresses the need for new austenitic steel compositions with higher creep strength and higher upper temperatures. The present invention also discloses a methodology for the development of new austenitic steel compositions with higher creep strengt...
12/02/2010
20100132598Corrosion Resistant Coatings Suitable For Elevated Temperature Application
The present invention relates to corrosion resistance coatings suitable for elevated temperature applications, which employ compositions of iron (Fe), chromium (Cr), nickel (Ni) and/or aluminum (Al). The compositions may be configured to regulate the diffusion of metals...
06/03/2010
20100116382AUSTENITIC STAINLESS STEEL EXCELLENT IN INTERGRANULAR CORROSION RESISTANCE AND STRESS CORROSION CRACKING RESISTANCE, AND METHOD FOR PRODUCING AUSTENITIC STAINLESS STEEL MATERIAL
An austenitic stainless steel excellent in intergranular corrosion resistance and stress corrosion cracking resistance, comprising: C: 0.005 wt % or less; Si: 0.5 wt % or less; Mn: 0.5 wt % or less; P: 0.005 wt % or less; S: 0.005 wt % or less; Ni: 15.0 to 40.0 wt %, Cr...
05/13/2010
20100062279Austenitic stainless steel welded joint and austenitic stainless steel welding material
An austenitic stainless steel welded joint, whose base metal and weld metal each comprises, by mass percent, C: not more than 0.3%, Si: not more than 2%, Mn: 0.01 to 3.0%, P: more than 0.04% to not more than 0.3%, S: not more than 0.03%, Cr: 12 to 30%, Ni: 6 to 55%, rar...
03/11/2010
20090285717Iron-Nickel-Chrome-Silicon-Alloy
Iron-nickel-chromium-silicon alloy having (in % by weight) 34 to 42% nickel, 18 to 26% chromium, 1.0 to 2.5% silicon, and additives of 0.05 to 1% Al, 0.01 to 1% Mn, 0.01 to 0.26% lanthanum, 0.0005 to 0.05% magnesium, 0.01 to 0.14% carbon, 0.01 to 0.14% nitrogen, max. 0....
11/19/2009
20090155119Weldable oxidation resistant nickel-iron-chromium-aluminum alloy
A weldable, high temperature oxidation resistant alloy with low solidification crack sensitivity and good resistance to strain age cracking. The alloy contains by weight percent, 25% to 32% iron, 18% to 25% chromium, 3.0% to 4.5% aluminum, 0.2% to 0.6% titanium, 0.2% to...
06/18/2009
20090129967FORGED AUSTENITIC STAINLESS STEEL ALLOY COMPONENTS AND METHOD THEREFOR
A forgeable austenitic stainless steel alloy and forging process capable of producing forged components that exhibit mechanical and environmental properties and metallurgical stability suitable for use in thermally and chemically hostile environments, such as the enviro...
05/21/2009
20090081074Wear resistant alloy for high temprature applications
Low cost alloys resistant to mechanical requirements related to high temperatures, resistant to corrosion, resistant to abrasion, with high workability and which meet different requirements in the conditions for application in either exhaust or intake valves for interna...
03/26/2009
20090068054Ti-Ni-Nb alloy device
To provide a Ti—Ni—Nb alloy device which is a shape memory device excellent in response characteristics.

The Ti—Ni—Nb alloy device is made of a Ti—Ni—Nb alloy which finishes transformation at a temperature lower than 10° C. aft...

03/12/2009
20090038280Stainless Steel For Filter Applications
A filter comprising a porous sintered stainless steel is provided. The filter includes 10-30% chromium, 5-25% nickel, 0.5-3% manganese; 1-4% silicon, and 0-3% molybdenum with the remainder being iron and inevitable impurities. The sintered steel has a density less than ...
02/12/2009
20080281401STAINLESS STEEL ALLOY HAVING LOWERED NICKEL-CHROMINUM TOXICITY AND IMPROVED BIOCOMPATIBILITY
The present invention is directed towards an austenitic, stainless steel series 300 alloy having improved biocompatible characteristics. The modified stainless steel alloy consists essentially of, in weight percent, about

11/13/2008

20080241580Filler Metal Composition and Method for Overlaying Low NOx Power Boiler Tubes
An alloy for use as a welding overlay for boiler tubes in a low NOx coal-fired boiler comprising in % by weight: 36 to 43% Cr, 0.2 to 5.0% Fe, 0-2.0% Nb, 0-1% Mo, 0.3 to 1% Ti, 0.5 to 2% Al, 0.005 to 0.05% C, 0.005 to 0.020% (Mg+Ca), 0-1% Mn, 0-0.5% Si, less ...
10/02/2008
20080159905Silicon alloy, alloy powder thereof, manufacturing apparatus, manufacturing process and sintered alloy thereof
A controlled combustion synthesis apparatus comprises an ignition system, a pressure sensor for detecting internal pressure, a nitrogen supply, a gas pressure control valve for feeding nitrogen and exhausting reaction gas, means for detecting the internal temperature of...
07/03/2008
 
Sign InRegister
Username  
Password   
forgot password?